● Performance
The imitation of the matte surface requires uniform metal powder in the coating, does not affect the module image function, the UV layer has a high light penetration, so that the solid pattern of the coating is perfectly fused with the exterior of the fingerprint module. Surface hardness is up to 4h
The high gloss has a mirror effect, and the ceramic / glass fitting panel can be achieved.
The UV lacquer surface can withstand the SMT back welding furnace 180 degrees for 3 minutes; matte UV paint surface can withstand the SMT back welding furnace 260 degree 3 minutes does not crack, no discoloration, crack, orange and other coatings;
Products can meet numerous first-line brand test requirements;